Mechanical bonding
To improve the bed adhesion and reduce warping of the first layer, several measures are available. For example, using a brim or raft that...
56 views
0 comments


Minimum cooling time
In a previous post the importance of controlling layer temperature is explained. In the latest prints poor results due to insufficient...
28 views
0 comments


The impact of layer height
The layer height is an important design parameter that impacts the printing time, cost, visual appearance and physical properties of a...
31 views
0 comments


Build plate adhesion
Since PP is known for its stubbornness to attach to other materials than itself, we were expecting some struggles with build plate...
22 views
0 comments


Controlling layer temperature
When 3D printing thermoplastic materials the controlling of layer temperature is of great importance to create quality prints. By...
14 views
0 comments


PP testing
Here are the results of the first tests with new recycled PP material from Eco-Oh! We are glad to have found we made the right decision...
51 views
0 comments


Overhang
Here are the test result of the overhang testing. With a layer height of 4 mm and overhang steps of 2 mm we managed to get good results...
7 views
0 comments


Nozzle isolation
By adding simple isolation around the nozzle we managed to increase the nozzle temperature from 60 up to 170 degree. Definitely one of...
29 views
0 comments

Household waste PE/PP
After many months of developing and testing to master the PE/PP material from household waste, our gathered data indicate that we will...
32 views
0 comments


Layer Bonding & Printing Height
Since the optimal layer height was found at 6.5 mm with a 5 mm nozzle, the layer bonding and printing height are up for the test....
17 views
0 comments


Layer Height
The optimal layer height will differ based on the output of a used nozzle. As starting point 80% of the nozzle size is valid in desktop...